Prefabricated lightened cement with industrial waste of polymeric origin and fiberglass in the form of a paver
Metadata
Show full item recordAuthor
Date
2023Subject/s
Abstract
1. Prefabricated cement lightened with industrial waste of polymeric origin and fiberglass, manufactured in the form of a paver for the production of flooring and other similar work units in building and civil engineering, with the following composition: - commercial cement; - arid; - crushed waste from recycled complete vehicle roofs, composed of a polymer matrix and fiberglass; - additives in a proportion of 0.8% with respect to the weight of the cement, and - water. 2. Prefabricated cement lightened with industrial waste of polymeric origin and fiberglass in the form of paving stone according to claim 1, characterized by an apparent density between 2150 kg/m 3 and 2180 kg/m 3 . 3. Prefabricated cement lightened with industrial waste of polymeric origin and fiberglass, in the form of a paver according to claims 1 and 2, characterized by a compression resistance between 3.8 MPa and 5.1 MPa. 4. Prefabricated cement lightened with industrial waste of polymeric origin and fiberglass, in the form of a paver according to any of claims 1 to 3, characterized by a resistance to breaking load with values between 420 N/mm and 565 N/mm. 5. Prefabricated cement lightened with industrial waste of polymeric origin and fiberglass, in the form of a paver according to any of claims 1 to 4, characterized by a resistance to wear due to abrasion between 14 and 17 mm. 6. Prefabricated cement lightened with industrial waste of polymeric origin and fiberglass, in the form of a paver according to any of claims 1 to 5, characterized by a total water absorption that is between 5.2% and 5. 9%. 7. Prefabricated cement lightened with industrial waste of polymeric origin and fiberglass, in the form of a paver according to any of claims 1 to 6, characterized by a slip resistance that is between 56 and 60 URSV. 8. Prefabricated cement lightened with industrial waste of polymeric origin and fiberglass, in the form of a paver according to any of claims 1 to 7, characterized by a Shore C surface hardness between 84 and 90. 9. Prefabricated of cement lightened with industrial waste of polymeric origin and fiberglass, in the form of a paver according to any of claims 1 to 8, characterized by having dimensions of (200x100x60) mm 3 .
1. Prefabricated cement lightened with industrial waste of polymeric origin and fiberglass, manufactured in the form of a paver for the production of flooring and other similar work units in building and civil engineering, with the following composition: - commercial cement; - arid; - crushed waste from recycled complete vehicle roofs, composed of a polymer matrix and fiberglass; - additives in a proportion of 0.8% with respect to the weight of the cement, and - water. 2. Prefabricated cement lightened with industrial waste of polymeric origin and fiberglass in the form of paving stone according to claim 1, characterized by an apparent density between 2150 kg/m 3 and 2180 kg/m 3 . 3. Prefabricated cement lightened with industrial waste of polymeric origin and fiberglass, in the form of a paver according to claims 1 and 2, characterized by a compression resistance between 3.8 MPa and 5.1 MPa. 4. Prefabricated cement lightened with industrial waste of polymeric origin and fiberglass, in the form of a paver according to any of claims 1 to 3, characterized by a resistance to breaking load with values between 420 N/mm and 565 N/mm. 5. Prefabricated cement lightened with industrial waste of polymeric origin and fiberglass, in the form of a paver according to any of claims 1 to 4, characterized by a resistance to wear due to abrasion between 14 and 17 mm. 6. Prefabricated cement lightened with industrial waste of polymeric origin and fiberglass, in the form of a paver according to any of claims 1 to 5, characterized by a total water absorption that is between 5.2% and 5. 9%. 7. Prefabricated cement lightened with industrial waste of polymeric origin and fiberglass, in the form of a paver according to any of claims 1 to 6, characterized by a slip resistance that is between 56 and 60 URSV. 8. Prefabricated cement lightened with industrial waste of polymeric origin and fiberglass, in the form of a paver according to any of claims 1 to 7, characterized by a Shore C surface hardness between 84 and 90. 9. Prefabricated of cement lightened with industrial waste of polymeric origin and fiberglass, in the form of a paver according to any of claims 1 to 8, characterized by having dimensions of (200x100x60) mm 3 .





